CUTTING SPEEDS THREADING

Recommended Starting Speeds v c (ft/min)

Brinell Hardness HB

Rockwell Hardness HRC

Tensile Strength MPa

ISO Material Group

Workpiece Material

S525 low start high

Gray Cast Iron Ex. Class 20, 25, 30, 35, 40, 45, 50, 55, 60, G1800, G3000, G3500, G4000

K1

120-290 <32 125-500 260 350 490

Ductile Cast Irons (Nodular Irons) and Compacted Graphite Irons (CGI) Ex. 60-40-18, 65-45-12, 80-55-06, SAE J434: D4018, D4512, D5506 High-Strength Ductile Irons and Austempered Ductile Irons (ADI) Ex. ASTM A536: 100-70-03, 120-90-02, SAE J434: D7003

K Cast Iron

K2

130-260 <28 <600 220 300 400

K3

180-350 <43

>600 200 260 320

Recommended Starting Speeds v c (ft/min)

Brinell Hardness HB

Rockwell Hardness HRC

Tensile Strength MPa

ISO Material Group

Workpiece Material

S525 low start high

Iron-Based Heat-Resistant Alloys Ex. A286, A608, INCOLOY 800 Series, N-155, Haynes 556, Discaloy

S1

160-260 25-48 500-1200 90 130 180

Cobalt-Based Heat-Resistant Alloys Ex. Haynes 25 (L605), Haynes 188, Stellite, MAR-M302, MAR-M509

S2

250-450 25-48 1000-1450 60 80 100

S High Temp Alloys

Nickel-Based Heat-Resistant Alloys

S3

160-450 <48 600-1700 45 60 80

Ex. Astroloy, Hastelloy X, INCONEL 600 and 700 Series, Waspalloy

Titanium and Titanium Alloys Ex. Commercially Pure Ti, Ti-5Al-2.5Sn, Ti-6Al-4V, Ti-3Al-8V-6Cr-4Zr-4Mo

S4

300-400 33-48 900-1600 165 200 230

83